No. 1 Temper Wire
Wire to AMS 5698 for springs that run hotter for longer.
Request Availability →Cold-drawn spring wire in No. 1 and spring tempers for coil and disc springs that run hot.
Inconel X-750 wire ships in No. 1 temper for hot duty and spring temper for highest tensile.
A coiled X-750 wire spring keeps most of its installed load after long hours at 650 °C.
We measure X-750 wire diameter on the drawing line, so the coil holds its band end to end.
Inconel X-750 wire ships in UNS N07750, a precipitation-hardening nickel-chromium-iron alloy. Titanium and aluminium build the gamma-prime precipitate inside this drawn wire. Niobium then slows its coarsening, so the wire keeps useful load at 704 °C.
We supply Inconel X-750 wire to AMS 5698 in No. 1 temper and to AMS 5699 in spring temper. Consequently, the ordered temper decides the tensile band of the wire, and we record it on the purchase order before drawing starts.
Meanwhile, the Inconel X-750 Bar and Rod hub also lists this wire beside the other forms. The European call-out NiCr15Fe7TiAl maps to the same UNS N07750 material as this wire.
Inconel X-750 wire is supplied in UNS N07750, the precipitation-hardening nickel-chromium-iron alloy strengthened by gamma prime. Titanium, aluminium and niobium build the precipitate that holds strength to 704 °C. Southerly Alloy supplies and exports X-750 wire to AMS 5698 and AMS 5699 in the No. 1 and spring tempers, with EN 10204 3.1 paperwork on every heat.
No. 1 temper wire carries the higher service temperature, and spring temper carries the higher tensile.
Specifically, a spring wound from X-750 wire keeps its installed load through long hot service.
Moreover, successive drawing passes raise the tensile band of the wire above the annealed floor.
Therefore, we gauge the wire at every drawing pass so the coil stays inside its band.
Each wire lot travels with the furnace chart for its own age at 732 or 649 °C.
In addition, we ship the wire on spools, in coils or as straightened cut lengths.
Each wire coil leaves on a spool with controlled tension.
In fact, a grain size reading travels with every spring temper wire lot.
Sourcing Inconel X-750 wire depends on matching the temper to the coiling step. Where the spring is formed after delivery, the softer No. 1 temper wire takes the bend without cracking.
Grade, wire diameter, temper and cycle enter the purchase order at the same time.
Consequently, each certificate records the drawing passes and the age applied to that wire heat.
In addition, a single wire spool proves the coiling behaviour before a production run.
Quotations for Inconel X-750 wire include the packing list, mill certificate and export documents.
One melt feeds every wire coil, and the ordered temper then sets the final properties. Because titanium and aluminium oxidise easily, melting control for X-750 wire matters as much as the drawing line.
Weighed nickel, chromium, iron, titanium and aluminium enter the melt that will become this wire order.
Vacuum induction melting holds titanium and aluminium inside a narrow window on every wire heat.
Consumable electrode or vacuum arc remelting follows, and the certificate records the route taken for the wire.
Forging and rolling reduce the ingot to wire rod above the recrystallisation temperature.
The rod is descaled and coated so the wire carries a clean surface into the dies.
Successive carbide dies pull the wire down to the ordered diameter, with in-line gauging at every pass.
The wire then ages at 732 °C for No. 1 temper or at 649 °C for spring temper.
Finally, we spool the wire and release it against the ordered tensile and diameter band.
Southerly Alloy supplies Inconel X-750 wire across the common drawn diameters and both AMS tempers. We confirm wire diameter, temper and coil weight against your order before production.
Melting, rod rolling, drawing and wire aging for Inconel X-750 wire sit inside one boundary.
Draw benches, spoolers, straighteners and gauges cover the wire sizes we stock.
Custom wire heats and stocked diameters share one campaign calendar.
A metallurgist reviews every X-750 wire enquiry before the offer leaves.
Chemistry and drawing decide these wire properties together, so our laboratory checks both. Therefore, the certificate reports the temper that produced the wire values.
The laboratory reads titanium, aluminium and niobium in the wire heat, then records each figure against the AMS table.
Specifically, tensile values for this wire come from the finished coil rather than from the rod.
In addition, we gauge wire diameter and ovality at the start, middle and end of every coil.
Consequently, every wire certificate carries the drawing and aging record for the same heat.
Different wire tempers suit different coiling and service needs. Therefore, the list below shows the Inconel X-750 Wire variants we quote most often.
Wire to AMS 5698 for springs that run hotter for longer.
Request Availability →Wire to AMS 5699 for the highest tensile band in a spring.
Request Availability →Solution-treated wire for springs that age after coiling.
Request Availability →Wire straightened and cut for cold-forming headers.
Request Availability →Soft wire for lockwire and safety wiring at temperature.
Request Availability →Custom Inconel X-750 wire produced against your own specification.
Request Availability →Coil springs and locking wire are where Inconel X-750 wire has served longest. Meanwhile, the engine trade relies on this drawn wire wherever installed load must survive the heat.
Discuss Your Application →Coil springs wound from X-750 wire that hold load at 650 °C.
Disc springs stacked from wire stock for hot assemblies.
Hold-down springs wound from wire inside the reactor vessel.
Safety wire that keeps fasteners locked through thermal cycling.
Wire rings that support metal bellows in hot gas lines.
Woven wire mesh for high-temperature screening.
Wire springs for duty well below −100 °C.
Wire springs and clips for thrust chamber hardware.
Detailed technical information including chemical composition, mechanical properties, standards and available dimensions.
The limits come from ASTM B637, which shares one composition table with the AMS documents for UNS N07750. Titanium and aluminium set the gamma-prime volume in this wire, while niobium slows its coarsening.
Iron balances the matrix, and the nickel plus cobalt floor keeps this wire austenitic. The full composition table on the Inconel X-750 material page lists every element against its ASTM limit.
The wire rows come from the AMS spring wire documents for UNS N07750. Diameter decides the applicable band, and the temper decides the aging cycle. Every value below is a minimum unless the row states a range.
| Product Form | Condition | Tensile Strength, min. | Yield Strength (0.2%), min. | Elongation, min. | Hardness |
|---|---|---|---|---|---|
| No. 1 temper wire, AMS 5698 | Cold drawn, aged at 732 °C for 16 h | 165-220 ksi (1138-1517 MPa) | - | - | - |
| Spring temper wire, AMS 5699 | Cold drawn, aged at 649 °C for 4 h | 180-250 ksi (1241-1793 MPa) | - | - | - |
| Spring temper wire, long cycle | Solution treated, stabilised, aged | 145-190 ksi (1000-1310 MPa) | - | - | - |
Wire diameters up to 0.64 mm follow their own tensile bands in the AMS documents. The drawn temper lifts tensile past the bar floor, and no further aging applies afterward.
Design work leans on the published figures for this grade, and density sits at 8.28 g/cm³. Moreover, the magnetic behaviour of this wire changes with the heat treatment applied, so the Curie temperature follows the cycle.
The physical properties table on the Inconel X-750 material page carries the remaining values, including the modulus and the thermal expansion.
Inconel X-750 wire is cold drawn and then aged, so the temper rather than a separate anneal sets its final strength. We supply the wire in the temper below that your spring needs.
| Temper | Typical Treatment |
|---|---|
| No. 1 temper | Cold drawn, then aged at 732 °C for 16 h |
| Spring temper | Cold drawn, then aged at 649 °C for 4 h |
| Long-cycle spring | Solution treated, stabilised, then aged |
| Soft (as-drawn) | Undrawn stock for buyers who age afterwards |
AMS 5698 and AMS 5699 are the wire documents for UNS N07750, while the bar and forging forms sit on ASTM B637. The three designations below settle most spring enquiries.
| Standard | Product or Application |
|---|---|
| AMS 5698 | Wire, No. 1 temper, precipitation hardenable |
| AMS 5699 | Wire, spring temper, precipitation hardenable |
| UNS N07750 - W.Nr. 2.4669 - NiCr15Fe7TiAl | Material designations |
The full standards list on the Inconel X-750 material page adds the AMS 5589 and AMS 5590 wire documents and the remaining bar numbers.
Pyromet X750, Nickelvac X750, Nicrofer 7016 TiNb, and Inconel are trademarks of their respective owners. We quote those names for reference only, and our deliveries follow the ASTM and AMS documents listed above.
The standard text from ASTM International settles any acceptance question.
Because AMS 5698 and AMS 5699 print their own scope, the wire ranges below follow those texts rather than one house rule. For that reason, state the wire diameter, the temper and the coil weight on the enquiry.
| Product Form | Typical Supply Range |
|---|---|
| No. 1 temper wire | 0.5-12 mm diameter in coils to AMS 5698 |
| Spring temper wire | 0.5-8 mm diameter in coils to AMS 5699 |
| Wire, straightened | Cut lengths for cold-forming headers |
| Wire, soft | Annealed stock for buyers who coil first and age afterwards |
Coils ship to the weight named on the order, and each AMS wire document settles its own diameter band. Therefore, fix the temper before the mill draws the coil.
Finish follows the operation that comes next rather than a catalogue default. Moreover, we agree the surface of this wire with your order.
| Surface Condition | Typical Use |
|---|---|
| Cold drawn | Close size control and a brighter surface on this wire. |
| Bright annealed | A scale-free surface on this wire for instrument and clean circuits. |
| Peeled | A machined skin gives this wire uniform diameter for further turning. |
Related forms from this heat cover rings, round bar and cold drawn bar.
Get detailed information including specifications, standards, dimensions and material properties.
Eight steps carry a wire enquiry from the first message to the delivered lot. Therefore, state the duty first, and the temper then follows from it.
Give the service temperature, the load and the medium that the wire spring will meet.
Tell us that the order is X-750 wire rather than bar, rod or plate.
We agree No. 1 temper or spring temper for the wire against that duty.
The quotation states the wire price per kilogram, the lead time and the certificate set.
Grade, wire diameter, temper and inspection level enter the order acknowledgement.
The melt shop weighs the charge and takes the wire heat through melting and remelting.
The wire passes the ordered drawing passes, the age and release testing.
Finally, the desk tracks the wire shipment and forwards the documents ahead of arrival.
Our production and inspection processes are certified to international standards, and every delivery ships with EN 10204 3.1 mill test certificates.
Quality Management System
Pressure Equipment Directive
Material Standards Compliance
Mill Test Certificates
ASTM B637 governs the bar, forging and ring forms of UNS N07750. In addition, the AMS 5667 group covers the same forms by melting route and solution treatment.
Type 2 suits wire below about 593 °C, because it carries the highest tensile floor at 1170 MPa. Above that temperature, the stabilised Type 1 cycle is the better choice.
No. 1 temper wire covers 0.5 to 12 mm diameter, and spring temper wire covers 0.5 to 8 mm diameter in coils.
Order No. 1 temper when the spring must run above 593 °C. For the highest tensile, order spring temper wire and finish the spring by grinding only.
It adds a stabilising hold near 843 °C after the solution treatment of the wire. Consequently, the Type 1 route protects creep life above 593 °C at some cost in tensile strength.
Yes. The AMS bar documents cover solution-treated and equalized conditions for buyers who machine the wire parts first and age them afterwards.
A single piece or one coil covers most stock sizes of wire, so a short cut is enough for a trial.
We quote wire mainly on FOB terms, and EXW or CIF follow on request.
Stock wire ships in 7 to 15 days, and made-to-order material runs about 25 days.
Yes. Every heat ships with an EN 10204 3.1 certificate, and we arrange 3.2 endorsement on request.
Send the wire diameter, the temper and the service temperature. The quotation carries the wire price, the lead time and the certificate set. Because the cycle decides the acceptance level for this wire, name the temper at enquiry.
A single X-750 wire coil proves the grade before a plant-wide commitment.